Please note that we are in the process of updating our websites. Our international (Non-Korean) websites will also be updated soon.
Please contact us for any inquiries (webadmin@anapro.com). Thank you.
1. TEM Image![]() |
2. Coating Layer SEM Image![]() Coating Method : Slot Die Coating |
Grade | Cure method | △T%(380-1100nm) | Pencil hardness |
Abrasion Resistance (400g felt) |
Boiling test (100˚C/10min) |
---|---|---|---|---|---|
AR250 | 300˚C, 30min | 3.01 | 3~4H | PASS | PASS |
250˚C,2min dry/ 700˚C,2min tempered |
|||||
AR750 | 250˚C,2min dry/ 700˚C,2min tempered |
3.04 | 3~4H | PASS | PASS |